When the plates were mounted to the rotary drum they sometimes had an excessive gap between the plates. When the gap was excessive they placed lead foil between the plates. This fiol made for a number of interesting joint lines. Sometimes the foil would fold over and produce a very irregular line and, as in this case, sometimes the foil would "roll out" smooth in the center and produce 2 lines at the very edges of the joint gap.
Disclaimer: While a tremendous amount of effort goes into ensuring the accuracy of the information contained in this site, Stamp Community assumes no liability for errors. Copyright 2005 - 2026 Stamp Community Family - All rights reserved worldwide. Use of any images or content on this website without prior written permission of Stamp Community or the original lender is strictly prohibited. Privacy Policy / Terms of UseAdvertise Here